Instructions:This tool will calculate the density of a solder given the constituent metal weight percentages. Simply put the weights percentages in the right hand column and the alloy density is displayed on the left. You must check to see that your weight percentages add up to 100%. If your alloy has a metal not listed, enter its density under "Other 1, 2, or 3".
References | |
SnPb Eutectic | 8.400 |
SAC305 | 7.360 |
SAC396 | 7.390 |
SnCu0.7 | 7.300 |